OS-CON DATA SHEET No.OS02N-DFSVP037 OS-CON 16SVP100M Frequency (kHz) Impedance (ohm) ESR (ohm) 0.12 13.49 0.31 0.5 3.29 0.10 1 1.66 0.07 10 0.178 0.038 100 0.035 0.028 500 0.023 0.022 1000 0.027 0.023 5000 0.082 0.024 10000 0.148 0.025 Frequency characteristics 1000 Impedance (ohm) ESR (ohm) ESR, Impedance (ohm) 100 10 1 0.1 0.01 0.001 0.1 1 10 100 1000 10000 Frequency (kHz) Measuring equipment: HP4194A Test fixture: HP16047C Measuring position: root of leads OS Engineering Department, OS-CON Control Department Saga SANYO Industries Co., Ltd. n = 3p.(Ave.) Room temperature OS-CON DATA SHEET SVP series Test item Endurance (After V.P.S test) Test temperature 105 deg.C Model Applied voltage 16 V Lot No. 16SVP100M 050901311 Tangent of loss angle (120Hz) Change in capacitance (120Hz) Tangent of loss angle 20 Percent delta [%] 10 0 -10 -20 -30 -40 2000 0 Time[h] ESR (100kHz) Leakage current (16V 60s) 10000 100 90 80 70 60 50 40 30 20 10 0 1000 100 10 1 0.1 0.01 0 2000 Time[h] Note: 2000 Time[h] Leakage current(A) ESR(mohm) 0 0.15 0.14 0.13 0.12 0.11 0.1 0.09 0.08 0.07 0.06 0.05 0.04 0.03 0.02 0.01 0 0 2000 Time[h] n =30p. Note: V.P.S test conditions : 230deg.Cx75sx2times (V.P.S = Vapor Phase Soldering method) Start on July 4, 2000 Executed by M. Koyama End on September 25, 2000 Drawn by S. Kodera No.OS02D-DESVP037 OS Engineering Department., OS-CON Control Department, Saga SANYO Industries Co., Ltd. OS-CON DATA SHEET SVP series Test item Damp heat (Steady state) (After V.P.S test) Test temperature 60 deg.C Model Test humidity 90 % RH Lot No. 16SVP100M 050901311 Change in capacitance (120Hz) Tangent of loss angle (120Hz) Tangent of loss angle 20 Percent delta [%] 10 0 -10 -20 -30 -40 1000 0 Time[h] ESR (100kHz) Leakage current (16V 60s) 100 90 80 70 60 50 40 30 20 10 0 10000 1000 100 10 1 0.1 0.01 0 1000 Time[h] Note: 1000 Time[h] Leakage current(A) ESR(mohm) 0 0.15 0.14 0.13 0.12 0.11 0.1 0.09 0.08 0.07 0.06 0.05 0.04 0.03 0.02 0.01 0 0 1000 Time[h] n =20p. Note: V.P.S test conditions : 230deg.Cx75sx2times (V.P.S = Vapor Phase Soldering method) Start on July 14, 2000 Executed by M. Koyama End on August 25, 2000 Drawn by M. Kimura No.OS02D-DHSVP037 OS Engineering Department, OS-CON Control Department, Saga SANYO Industries Co., Ltd.