SPECIFICATION * Supplier : Samsung electro-mechanics * Product : Multi-layer Ceramic Capacitor * Part Number : * Description : CL32F475ZAHNNNE CAP, 4.7 , 25V, -20/+80%, Y5V, 1210 A. Samsung Part Number Series Size Dielectric Capacitance Capacitance tolerance Rated Voltage Thickness CL 32 F 475 Z A H N N N E Samsung Multi-layer Ceramic Capacitor 1210 (inch code) L: 3.2 0.3 2.5 W: Inner electrode Termination Y5V 4.7 -20/+80 % mm 0.2 mm Ni Cu Sn 100% Plating 25 V 1.6 0.2 mm (Pb Free) Product Special Normal Packaging Embossed Type, 7" reel Reserved for future use B. Samsung Reliablility Test and Judgement condition Performance 1.00.2Vrms Rated Voltage 60~120 sec. Resistance 10,000Mohm or 100Mohm Whichever is Smaller Appearance No abnormal exterior appearance Withstanding No dielectric breakdown or Microscope (x10) 250% of the rated voltage Voltage mechanical breakdown Temperature Y5V Characterisitcs Adhesive Strength (From -30 to 85, Capacitance change shoud be within -82~+22%) No peeling shall be occur on the 500gF, for 101 sec. of Termination terminal electrode Bending Strength Capacitance change : Tan (DF) Insulation Within specified tolerance Test condition 110% Capacitance 0.07 max. within 30% Bending to the limit (1mm) with 1.0mm/sec. Solderability More than 75% of terminal surface SnAg3.0Cu0.5 solder is to be soldered newly 2455, 30.3sec. (preheating : 80~120 for 10~30sec.) Resistance to Capacitance change : Soldering heat Tan , IR : initial spec. within 20% Solder pot : 2705, 101sec. Performance Vibration Test Capacitance change : within 20% Test condition Amplitude : 1.5mm Tan , IR : initial spec. From 10 to 55 (return : 1min.) Moisture Capacitance change : 2hours x 3 direction (x, y, z) With rated voltage Resistance Tan : IR : High Temperature Resistance 0.09 max Tan : 402, 90~95%RH, 500+12/-0hrs 500Mohm or 25Mohm Whichever is Smaller Capacitance change : IR : within 30% within 30% 0.09 max Capacitance change : Cycling Tan , IR : initial spec. of the rated voltage Max. operating temperature 1000Mohm or 50Mohm Whichever is Smaller Temperature With 200% within 20% 1000+48/-0hrs 1 cycle condition Min. operating temperature 25 Max. operating temperature 25 5 cycle test C. Recommended Soldering method : Reflow ( Reflow Peak Temperature : 260+0/-5, 10sec. Max ) * For the more detail Specification, Please refer to the Samsung MLCC catalogue.