GT15
Thermal Conductivity
Glassber Reinforcement
Smooth surface & low thermal contact resistance
Exceptional thermal performance at lower application pressures (20psi~400psi)
Usable over a wide temperture range
Electrically isolating
Complies with UL standards
High Thermal Conductivity Glassber Reinforcement is guaranteed against detachment, under normal use, for 5 years from the purchase date.
User shall be solely responsible for determining the suitability of TIM for the intended use, and the user assumes all risks and liabilities whatsoever
in connection there with. Neither seller nor manufacturer shall be liable either in tort or in contract for any loss damage, including loss of prots or
revenue arising out of the use or the inability to use a product.
Features
Properties
Limited Warranty
Property GT15 Unit Test Method
Colour Yellow - Visual
Reinforcement Fiberglass - -
Thickness 0.23 (mm) -
Op. Temp. Range -45 to 180 ˚C -
Density 2.35 g/cm3ASTM D792
Thermal Conductivity 1.5 W/mK ASTM D5470
Hardness 75 Shore A ASTM D2240
Breakdown Voltage AC 4000 V ASTM D149
Breakdown Voltage DC 6000 V ASTM D149
Dielectric Constant 5.8 1000 Hz ASTM D150
Thermal Impedance ˚C in 2/W
t=0.23mm 20psi 0.70 psi ASTM D5470
t=0.23mm 50psi 0.61 psi ASTM D5470
t=0.23mm 100psi 0.49 psi ASTM D5470
t=0.23mm 200psi 0.43 psi ASTM D5470
t=0.23mm 400psi 0.40 psi ASTM D5470
TML ‹ 0.2 % % ASTM E595
Tensile Strength 200 psi ASTM D412
Elongation 60 % ASTM D412
UL Flammability V-0 - UL 94
Tel: +44 20 8133 2062 Email: sales@tglobaltechnology.com Web: www.tglobaltechnology.com Skype: tglobal.technology